PRODUCT
SAFETY
Any fitting or fabrication work should be carried out in accordance with applicable site safety standards, ensuring use of approved hard hats, eye protection, steel-toed shoes and protective gloves. Always use a soft faced hammer when performing the work as described in these instructions.
WELDING PROCEDURE
CAUTION: Temperature must not exceed 392°F. Excessive heat input may cause cracking and delamination. Use suitably calibrated device to monitor temperature. Do not weld continuously. Continuous weld may cause warping, delamination, and cracking.
Ensure that the Laminite® backing plate and mating metal surface is clean and flat
Contact a CR representative for the appropriate procedure
Clamp and tack weld Laminite® into position
Stitch weld, laying 1.97” maximum length on each run, alternating ends or sides to minimize heat input
Do not deposit weld within 2mm from joint line between Laminite® and steel backing plate, as shown.